| CPC C08L 23/12 (2013.01) [C08L 23/06 (2013.01)] | 19 Claims |
|
1. A polymer composition comprising at least the following components
A) 20 to 55 wt.-% based on the overall weight of the polymer composition of a polymer blend, comprising
a1) polypropylene; and
a2) polyethylene;
wherein the weight ratio of a1) to a2) is from 1:1 to 12:1; and
wherein the polymer blend A) is a recycled material; and
B) 45 to 80 wt.-% based on the overall weight of the polymer composition of a virgin polypropylene homopolymer; wherein said virgin polypropylene homopolymer has
a MFR2 (230° C., 2.16 kg) determined according to ISO 1133 in the range of 15 to 35 g/10 min;
a xylene soluble content (XCS) determined according to ISO 16152, 1 ed, 25° C., based on the overall weight of component B) in the range of 1.0 to 3.0 wt.-%; and
a melt peak temperature measured according to ISO 11357 in the range of 150 to 170° C.;
with the proviso that the weight proportions of components A) and B) add up to 100 wt.-%.
|