US 12,729,276 B2
Method of preparing superabsorbent polymer
Junwye Lee, Daejeon (KR); Chang Hun Han, Daejeon (KR); Tae Young Won, Daejeon (KR); Jungmin Sohn, Daejeon (KR); Hyemin Lee, Daejeon (KR); Jihye Ryu, Daejeon (KR); and Minsu Kim, Daejeon (KR)
Assigned to LG Chem, Ltd., Seoul (KR)
Appl. No. 17/796,055
Filed by LG Chem, Ltd., Seoul (KR)
PCT Filed Aug. 17, 2021, PCT No. PCT/KR2021/010870
§ 371(c)(1), (2) Date Jul. 28, 2022,
PCT Pub. No. WO2022/080641, PCT Pub. Date Apr. 21, 2022.
Claims priority of application No. 10-2020-0134425 (KR), filed on Oct. 16, 2020.
Prior Publication US 2023/0119016 A1, Apr. 20, 2023
Int. Cl. C08J 3/075 (2006.01); C08J 3/12 (2006.01); C08J 3/24 (2006.01)
CPC C08J 3/075 (2013.01) [C08J 3/12 (2013.01); C08J 3/245 (2013.01); C08J 2323/04 (2013.01)] 4 Claims
 
1. A method of preparing a superabsorbent polymer, the method comprising:
1) Carrying out a crosslinking polymerization of a monomer composition comprising a water-soluble ethylene-based unsaturated monomer having acidic groups which are at least partially neutralized, in the presence of a foaming agent, to form a water-containing gel polymer;
2) Gel-pulverizing the water-containing gel polymer;
3) Drying, pulverizing, and size-sorting the gel-pulverized water-containing gel polymer to form a base polymer powder; and
4) Carrying out a surface crosslinking of the base polymer powder by heat treatment in the presence of a surface crosslinking agent,
wherein the foaming agent is present in an amount of 500 to 1,500 ppm in the monomer composition, and
the gel-pulverizing is carried out by extruding the water-containing gel polymer through a perforated panel having a plurality of holes using a screw extruder mounted inside a cylindrical pulverizer under a condition that a chopping index according to Equation 1 is 60 to 75:

OG Complex Work Unit Math
wherein in Equation 1,
N represents a number of rotation (rpm) of a screw in the screw extruder,
A represents porosity (πr2×n/πR2) of the perforated panel, wherein r represents a radius (mm) of the holes formed in the perforated panel, n represents a number of holes formed in the perforated panel, and
R represents a radius (mm) of the perforated panel,
wherein the superabsorbent polymer has a CRC of 27 g/g to 40 g/g as measured in accordance with EDANA WSP 241.3,
a AUP of 24 g/g to 30 g/g as measured in accordance with EDANA WSP 242.3,
a vortex of 40 seconds or less as measured by adding 2 g of the superabsorbent polymer to 50 mL of physiological saline at 23° C. to 24° C., and stirring with a magnetic bar (diameter of 8 mm and length of 31.8 mm) at 600 rpm, and a time taken for vortex to disappear being measured in seconds, and
a permeability of 30 to 60 seconds measured according to Equation 4:

OG Complex Work Unit Math
wherein in Equation 4,
Perm represents permeability of the superabsorbent polymer, T1 represents a time (sec) taken for 20 mL of a physiological saline solution (0.9% by weight of aqueous sodium chloride solution) to pass through the swollen superabsorbent polymer under a pressure of 0.3 psi, after placing 0.2 g of the superabsorbent polymer in a cylinder, and pouring the physiological saline solution whereby the superabsorbent polymer was completely submerged therein to allow the superabsorbent polymer to swell for 30 minutes.