| CPC C08G 73/1067 (2013.01) [C08G 73/1032 (2013.01); C08J 5/18 (2013.01); C08J 9/0066 (2013.01); C08J 9/286 (2013.01); C08K 9/02 (2013.01); H05K 9/0081 (2013.01); C08J 2201/0502 (2013.01); C08J 2205/044 (2013.01); C08J 2379/08 (2013.01)] | 15 Claims |

|
1. A manufacturing method of a porous polyimide film, the method comprising: preparing a polyamic acid solution at a concentration of 10 to 30 wt % by dissolving a diamine compound and a dianhydride in a solvent and adding a porous inorganic filler;
applying the prepared polyamic acid solution to a substrate to prepare a film and then immersing the same in a non-solvent for 30 minutes to 180 minutes; and
taking out the immersed film and thermally curing the same, wherein the porous inorganic filler is selected from the group consisting of mesoporous silica of MCM-41 or MCM-48; polyhedral oligomeric silsesquioxane (POSS); and zeolite of zeolite X or zeolite Y.
|