US 12,729,135 B2
Positive electrode active material for lithium secondary battery and method of preparing the same
Sang Min Park, Daejeon (KR); Eun Sol Lho, Daejeon (KR); Sung Bin Park, Daejeon (KR); Seul Ki Kim, Daejeon (KR); Wen Xiu Wang, Daejeon (KR); Joong Yeop Do, Daejeon (KR); and Wang Mo Jung, Daejeon (KR)
Assigned to LG Energy Solution, Ltd., Seoul (KR)
Appl. No. 17/788,814
Filed by LG Energy Solution, Ltd., Seoul (KR)
PCT Filed Jan. 29, 2021, PCT No. PCT/KR2021/001219
§ 371(c)(1), (2) Date Jun. 24, 2022,
PCT Pub. No. WO2021/154035, PCT Pub. Date Aug. 5, 2021.
Claims priority of application No. 10-2020-0011339 (KR), filed on Jan. 30, 2020.
Prior Publication US 2023/0034497 A1, Feb. 2, 2023
Int. Cl. H01M 4/525 (2010.01); H01M 4/02 (2006.01); H01M 4/04 (2006.01); H01M 4/485 (2010.01); H01M 4/505 (2010.01); H01M 10/052 (2010.01)
CPC H01M 4/525 (2013.01) [H01M 4/0471 (2013.01); H01M 4/485 (2013.01); H01M 4/505 (2013.01); H01M 10/052 (2013.01); H01M 2004/021 (2013.01); H01M 2004/028 (2013.01)] 11 Claims
 
1. A positive electrode active material, comprising:
a lithium transition metal oxide having nickel (Ni) in an amount of greater than 50 mol % based on a total number of moles of transition metals in the lithium transition metal oxide, wherein the transition metals exclude lithium,
wherein the positive electrode active material is in a form of single particles,
wherein a single particle has a region of 50 nm or less from a surface of the single particle along a center direction, and wherein a structure belonging to space group FD3-M and a structure belonging to space group Fm3m are formed in the region,
wherein a generation rate of fine powder having an average particle diameter (D50) of 1 μm or less is in a range of 5% to 30% when the positive electrode active material is rolled at 650 kgf/cm2,
wherein the positive electrode active material has a formation ratio of 0.2 to 0.7, where the formation ratio is the length of the structure belonging to space group FD3-M in the region to the length of the structure belonging to space group Fm3m in the region, where each length is measured along the center direction, and
wherein the lithium transition metal oxide is represented by Formula 1:
Li1+aNixCoyMnzM1wO2  [Formula 1]
wherein, in Formula 1,
M1 is at least one selected from the group consisting of aluminum (Al), magnesium (Mg), vanadium (V), titanium (Ti), and zirconium (Zr), and
0≤a≤0.20, 0.5<x<1.0, 0<y<0.5, 0<z<0.5, 0≤w≤0.05, and x+y+z+w=1.