| CPC C01B 32/174 (2017.08) [C01B 32/162 (2017.08); C09D 7/20 (2018.01); C09D 7/61 (2018.01); C09D 7/70 (2018.01); C09D 17/002 (2013.01); C09D 17/004 (2013.01); H01G 11/36 (2013.01); H01G 11/86 (2013.01); H01M 4/625 (2013.01); B82Y 30/00 (2013.01); B82Y 40/00 (2013.01); C01B 2202/22 (2013.01); C01B 2202/32 (2013.01); C01B 2202/36 (2013.01); C01P 2004/03 (2013.01); C01P 2006/22 (2013.01); C08K 3/041 (2017.05); C08K 2201/003 (2013.01); C08K 2201/006 (2013.01); C08K 2201/011 (2013.01)] | 6 Claims |

|
1. A method for preparing a carbon nanotube dispersion, comprising:
preparing a carbon nanotube bundle;
post-processing the carbon nanotube bundle to reduce an average length of the carbon nanotube bundle to 50 μm or less; and
dispersing the carbon nanotube bundle in a solution, wherein a volume-based particle size Dv (90) of the carbon nanotube bundle is 50 μm or less,
wherein the solution includes a solvent and a dispersant,
wherein the solvent is at least one of deionized water, N-methyl-2-pyrrolidone, or a combination thereof,
wherein the dispersant is at least one of polyvinylpyrrolidone, hydrogenated nitrile rubber, or a combination thereof,
wherein the dispersing is performed using a bead mill,
wherein the post-processing is performed by dry milling using an air dry mill,
wherein a saturation point according to a dispersion energy of a viscosity (μ) of the carbon nanotube dispersion is proportional to an average length value of the carbon nanotube bundle, and
wherein the viscosity of the carbon nanotube dispersion increases and then becomes saturated as the dispersion energy increases.
|