| CPC B27K 5/007 (2013.01) [B27D 1/04 (2013.01); B27K 3/0278 (2013.01); B27K 5/001 (2013.01); B27K 5/0095 (2013.01); B27K 5/065 (2013.01); G06K 19/07722 (2013.01)] | 18 Claims |

|
1. A method for producing a laminated structure comprising the steps of:
a) densifying a layer of hygroscopic material comprising a natural hygroscopic material or wood, the densifying comprising:
i) providing the hygroscopic material to be densified;
ii) pre-conditioning of the hygroscopic material by adjusting the moisture content of the hygroscopic material to a value within a predefined moisture range, if required;
iii) simultaneously heating and pressing the hygroscopic material under predefined temperature and pressure conditions, wherein the moisture content of the hygroscopic material is kept constant; and
iv) obtaining a densified material,
wherein:
the layer of the hygroscopic material is densified in said method step of densifying a hygroscopic material, and afterwards laminated with at least one further layer, wherein the at least one further layer comprising at least one of:
(i) another layer of hygroscopic material that was densified according to said method step of densifying a hygroscopic material; and/or;
(ii) plant-based material, animal-based material and/or wood-based material comprising paper, plant and/or wood fibers, wood-chips, wood flour, cellulose, starch, lignin, wood bark, wood extractives, algae, chitin-based materials, chitosan-based materials, native wood, protein, coal, char, carbon black and/or active coal; and/or;
(iii) metals and/or metal alloys comprising Aluminum, Steel, Copper, Silver, Gold, and/or Titanium; and/or;
(iv) polymeric materials comprising synthetic polymers and/or biopolymers, e.g. PLA, PET, PP, PE, PVC and/or proteins; and/or; and
(v) inorganic materials selected from ceramics, glass, stone, clay, metal-organic frameworks, zeolites, coal, char, carbon black and/or active coal; or other porous or non-porous inorganic materials,
wherein the laminated structure is produced such that the laminated structure comprises:
a) a backside made of a layer of a densified or non-densified wood veneer;
b) a frontside made of a layer of a densified or non-densified wood veneer; and
c) an integrated circuit, a memory device, a tracking device, a sensing device, an antenna and/or an electromagnetic coil,
wherein the layers are laminated and at least one of the layers of wood veneer is made of densified wood veneer, and
wherein the densification step comprises the following sub-steps:
iii1) the hygroscopic material is pre-heated to a first temperature at a first pressure and kept for a predefined first dwell time, wherein, the first pressure is equal to ambient pressure;
iii2) while keeping the first temperature, the pressure is raised to a second pressure, at a constant rate of pressure increase, and kept for a predefined second dwell time;
iii3) while keeping the second pressure, the temperature is increased to a second temperature, at a constant rate of temperature increase, and kept for a predefined third dwell time;
iii4) reducing the temperature to room temperature; and
iii5) reducing the pressure to ambient pressure.
|