US 12,728,181 B2
Solution blow spun polymer constructs, compositions and methods of fabrications and uses relating thereto
John Daristotle, Bel Air, MD (US); Shadden Zaki, Bethesda, MD (US); Peter Kofinas, North Bethesda, MD (US); Anthony Sandler, Bethesda, MD (US); Lung Lau, Washingtron, DC (US); and Leopoldo Torres, Greenbelt, MD (US)
Assigned to University of Maryland, College Park, College Park, MD (US); and Children's National Medical Center, Washington, DC (US)
Appl. No. 17/437,280
Filed by University of Maryland, College Park, College Park, MD (US); and Children's National Medical Center, Washington, DC (US)
PCT Filed Mar. 10, 2020, PCT No. PCT/US2020/021879
§ 371(c)(1), (2) Date Sep. 8, 2021,
PCT Pub. No. WO2020/185771, PCT Pub. Date Sep. 17, 2020.
Claims priority of provisional application 62/816,568, filed on Mar. 11, 2019.
Prior Publication US 2022/0160929 A1, May 26, 2022
Int. Cl. A61L 24/00 (2006.01); A61L 24/04 (2006.01); A61L 26/00 (2006.01)
CPC A61L 24/0015 (2013.01) [A61L 24/0073 (2013.01); A61L 24/046 (2013.01); A61L 26/0019 (2013.01); A61L 26/0066 (2013.01); A61L 26/0076 (2013.01)] 14 Claims
OG exemplary drawing
 
1. A composition comprising:
a solution comprising:
(i) between about 1% and about 20% weight per volume (w/v) low molecular weight (LMW) polymer; and (ii) between about 1% and about 20% (w/v) high molecular weight (HMW) polymer;
wherein said LMW polymer is PEG;
wherein said poly(ethylene glycol) (PEG) has a molecular weight of 950 to 1050 Da; and
wherein said HMW polymer has a molecular weight of about 10000 Da to about 42000 Da.