| CPC C09K 8/493 (2013.01) [C04B 7/13 (2013.01); C04B 7/40 (2013.01); C04B 7/522 (2013.01); C04B 7/527 (2013.01); C04B 28/02 (2013.01); C09K 8/426 (2013.01); E21B 33/13 (2013.01); C04B 2111/00275 (2013.01); C04B 2111/00663 (2013.01); C04B 2111/22 (2013.01)] | 13 Claims |

|
1. A method of cementing, comprising the steps of:
a) obtaining a cementitious composition comprising basalt powder (BP) as a supplementary cementitious material (SCM) in dry base cement powder, wherein the basalt powder comprises a particle size equivalent to the fraction passing through a #325 mesh sieve, up to 0.044 mm and 4000-6000 m2/kg;
b) mixing the cementitious composition with water and optional additives to form a hydraulic cementitious composition; and
c) performing primary cementing, secondary cementing, recovery, and/or plugging of a subsurface reservoir, using the hydraulic cementitious composition.
|