| CPC C01B 21/0648 (2013.01) [C04B 35/583 (2013.01); C04B 35/62802 (2013.01); C04B 35/62884 (2013.01); H05H 1/2406 (2013.01); C01P 2004/04 (2013.01); H05H 2245/40 (2021.05)] | 8 Claims |

|
1. A method for water-repellent treatment of boron nitride powders, the method comprising the steps of:
performing plasma treatment on the boron nitride powders by injecting a vaporized silicon-containing organic compound into a plasma generated region using a dielectric barrier discharge plasma apparatus;
wherein the injection of the vaporized silicon-containing organic compound includes passing a solution of the silicon-containing organic compound through a bubbler, and injecting the vaporized silicon-containing organic compound and a carrier gas into the plasma generated region;
wherein the plasma includes plasma formed from the silicon-containing organic compound;
wherein performing the plasma treatment includes forming a water-repellent coating layer on surfaces of the boron nitride powders;
wherein the silicon-containing organic compound includes hexamethyldisiloxane, tetraethoxysilane (TEOS) or trimethylchlorosilane (TMCS);
wherein the water-repellent coating layer contains silicon, carbon and oxygen; and
wherein the water-repellent coating layer chemically bonds to the boron nitride.
|