CPC D01F 6/84 (2013.01) [C08G 63/183 (2013.01); C08G 63/6856 (2013.01); C08G 63/80 (2013.01); C08G 63/866 (2013.01); C08G 63/916 (2013.01); D01D 5/08 (2013.01); D01F 11/08 (2013.01); D10B 2331/04 (2013.01); D10B 2401/063 (2013.01)] | 11 Claims |
1. A thermal-stability polyester industrial yarn, comprising polyester, wherein the polyester comprises a terephthalic acid, an ethylene glycol and a 2,6-pyridinedicarboxylic acid, and wherein 2,6-pyridinedicarboxylic acid is coordinated by an Fe3+ coordination agent;
wherein a molar ratio of the terephthalic acid to the 2,6-pyridinedicarboxylic acid is 1:(0.03-0.05);
wherein O atoms on two carbonyl groups and N atoms of the 2,6-pyridinedicarboxylic acid are involved in the coordination;
wherein a coordination structure formed between the Fe3+ coordination agent and the 2,6-pyridinedicarboxylic acid is:
wherein a glass transition temperature of the thermal-stability polyester industrial yarn is 88-92° C.,
wherein the thermal-stability polyester industrial yarn is formed by soaking wound fibers in an aqueous solution of the coordination agent at 80-100° C. for 48-72 hours, and a concentration of the aqueous solution of the coordination agent is 0.1-0.2 mol/L; and
wherein the coordination agent is FeCl3, Fe(NO3)3 or Fe2(SO4)3.
|