CPC C08F 4/78 (2013.01) [C08F 4/025 (2013.01)] | 23 Claims |
1. A process for preparing a titanated silica support, the process comprising:
(i) contacting water, hydrogen peroxide, an alkali metal precursor and/or a zinc precursor, a titanium precursor, and a silica to form a first mixture;
(ii) contacting the first mixture with a nitrogen-containing compound to form a second mixture;
(iii) subjecting the second mixture to a reaction temperature in a range from 40 to 270° C.;
(iv) isolating a solid fraction from the second mixture and washing the solid fraction; and
(v) drying the solid fraction to form the titanated silica support.
|