CPC C08F 232/06 (2013.01) [C08F 212/08 (2013.01); C09J 125/08 (2013.01); C09J 145/00 (2013.01); C08F 8/04 (2013.01); C08F 2500/02 (2013.01); C08F 2500/22 (2013.01)] | 17 Claims |
1. A method for manufacturing a hydrocarbon resin comprising at least one cyclic diolefin monomer component and at least one ethylenically unsaturated aromatic monomer component comprising
(a) heating to a temperature of at least 180° C. at a heating rate of 0.5 to 10° C./second a mixture comprising at least one cyclic diolefin monomer component and at least one ethylenically unsaturated aromatic monomer component having 8-13 carbon atoms, and
(b) polymerizing the mixture to form a hydrocarbon resin having a molecular weight of less than 2,500 g/mol, the molecular weight characterized as the centrifuge average (z-average) molecular weight,
wherein the mixture comprises a single phase liquid during heating and polymerization.
|