CPC H01M 4/505 (2013.01) [C01G 45/1228 (2013.01); C01P 2002/52 (2013.01); C01P 2002/72 (2013.01); C01P 2004/03 (2013.01); C01P 2006/40 (2013.01); H01M 2004/028 (2013.01)] | 20 Claims |
1. A method comprising:
mixing a lithium compound with a metal precursor compound comprised of Mn having an oxidation state of 2, wherein at least 50% by weight of the Mn has an oxidation state of 2 to form a mixture and heating the mixture to a temperature to form a disordered rocksalt.
|