| CPC C08L 67/02 (2013.01) [B32B 7/12 (2013.01); B32B 27/08 (2013.01); B32B 27/32 (2013.01); C08K 3/36 (2013.01); C08L 33/08 (2013.01); B32B 2250/242 (2013.01); B32B 2255/10 (2013.01); B32B 2255/26 (2013.01); B32B 2255/28 (2013.01); B32B 2264/1021 (2020.08); B32B 2307/518 (2013.01); B32B 2307/704 (2013.01); B32B 2307/75 (2013.01); B32B 2519/00 (2013.01)] | 20 Claims |

|
1. A film comprising:
a base layer comprising a biaxially oriented polypropylene (BOPP);
a coating layer comprising a polyester, an acrylic, and a crosslinker; and
a primer;
wherein the film has a haze change, measured according to ASTM D1003, before exposure to boiling water for 30 minutes and after an exposure to boiling water for 30 minutes of 4 units or less;
wherein according to FTIR the film has a first absorbance at a first wavelength of 1380 cm−1 higher than a second absorbance at a second wavelength of 1150 cm−1 and a third absorbance at a third wavelength of a 1450 cm−1 wavelength; and
wherein the third absorbance is higher than a fourth absorbance at a fourth wavelength of 1730 cm−1.
|