1. A method for green and low-cost extraction of nickel-cobalt from laterite nickel ore, comprising the following steps:
(1) iron removing pretreatment: adding an iron removing agent to a high-pressure leaching solution of the laterite nickel ore to reduce an iron concentration to less than 0.2 g/L to obtain a laterite nickel ore leaching solution;
(2) nickel adsorption: adsorbing and enriching nickel in the laterite nickel ore leaching solution using a first resin adsorption process to obtain a nickel adsorption resin and a nickel adsorption tail liquid; wherein the nickel adsorption resin is desorbed to obtain a crude nickel solution;
(3) cobalt adsorption: subjecting the nickel adsorption tail liquid to cobalt adsorption and enrichment by a second resin adsorption process and to obtain a cobalt solution by desorbing; and
(4) copper adsorption: subjecting the crude nickel solution to a third resin adsorption process for removing copper to obtain a purified nickel solution.
|