1. A method of preparing processed silk fibroin and controlling hydrolysis of silk fibroin, comprising
providing raw silk,
degumming the raw silk in 0.5 M sodium carbonate at a temperature of 80 to 90° C., and for a time of 120 to 480 minutes, to provide degummed silk fibers,
dissolving the degummed silk fibers in 5 to 13 M lithium bromide at a concentration of 10% (w/v) to 30% (w/v), and
removing the lithium bromide by Tangential Flow Filtration to provide the processed silk fibroin,
wherein the combination of sodium carbonate concentration, time and temperature of the degumming control the hydrolysis of the silk fibroin, and
wherein the processed silk fibroin has an average molecular weight of 15 kDa to 55 kDa by HPLC SEC using a Waters BEH200 Protein Standard Mix.
|