CPC C08H 6/00 (2013.01) [C08L 97/005 (2013.01)] | 16 Claims |
1. A method for preparing a lignin dispersion comprising the steps of
a) providing an aqueous medium having a pH of 1 to 7;
b) adding lignin to the aqueous medium, wherein the lignin is added in a form of a slurry having a solid content of lignin in a range of from 30 wt-% to 95 wt-%, calculated based on a total weight of the slurry; and,
c) mixing the aqueous medium until a dispersion of lignin in the aqueous medium has been obtained,
wherein steps a), b), and c) are carried out without actively heating the aqueous medium,