CPC C08L 27/20 (2013.01) [B29C 45/0001 (2013.01); C08K 3/38 (2013.01); C08L 27/18 (2013.01); B29K 2027/18 (2013.01); C08K 2003/385 (2013.01); C08K 2201/005 (2013.01)] | 9 Claims |
1. A resin composition comprising a fluororesin and boron nitride particles,
the fluororesin being present in an amount of 35 to 70% by mass and the boron nitride particles being present in an amount of 30 to 65% by mass, each relative to the resin composition,
the resin composition having a melt flow rate of 5.0 g/10 min or more,
wherein the boron nitride particles have a 90% particle size (D90) of 5.0 μm to 9.0 μm.
|