CPC C08F 220/18 (2013.01) [C10M 145/14 (2013.01); C10M 2203/1025 (2013.01); C10M 2209/084 (2013.01); C10N 2020/02 (2013.01); C10N 2020/04 (2013.01); C10N 2030/68 (2020.05)] | 17 Claims |
1. A method for the preparation of a polyalkyl (meth)acrylate polymer having a weight-average molecular weight in a range of 100,000 to 1,000,000 g/mol and comprising the following monomers:
(a) 8 to 25% by weight of at least one ester of (meth)acrylic acid and hydroxylated hydrogenated polybutadiene;
(b1) 60% to 80% by weight of at least one C1-4 alkyl (meth)acrylate;
(b2) 10% to 20% by weight of at least one C10-30 alkyl (meth)acrylate; and
(b3) 0% to 10% by weight of styrene;
based on a total amount of the polyalkyl (meth)acrylate polymer,
the method comprising:
(i) preparing a monomer mixture 1 comprising 115 to 125% of a targeted content of monomer 1(a) and 95% to 100% of a targeted content of monomers (b1) to (b3), a concentration of the monomers (a) to (b3) in monomer mixture 1 being 30 to 40%;
(ii) adding a monomer mixture 2 comprising 115 to 125% of the targeted content of monomer (a) and 95% to 100% of the targeted content of monomers (b1) to (b3), a concentration of the monomers (a) to (b3) in monomer mixture 2 being 30 to 40%; and
(iii) adding a monomer mixture 3 comprising 110 to 120% of the targeted content of only monomers (b1) to (b3), the concentration of the monomers (b1 to (b3) in monomer mixture 3 being 2 to 6%,
wherein monomer mixture 1 comprises 38 to 45% of a total amount of monomers used in the method, monomer mixture 2 comprises 38 to 45% of the total amount of monomers used in the method, and monomer mixture 3 comprises 15 to 20% of the total amount of monomers used in the method.
|