| CPC H01M 4/505 (2013.01) [H01M 4/0471 (2013.01); H01M 4/362 (2013.01); H01M 4/366 (2013.01); H01M 4/525 (2013.01); H01M 10/0525 (2013.01); H01M 2004/021 (2013.01); H01M 2004/028 (2013.01)] | 3 Claims |

|
1. A method for evaluating a characteristic of a positive electrode active material for non-aqueous electrolyte secondary batteries,
the characteristic being a “slurry pH” indicating a pH of a slurry containing water and the positive electrode active material as a solid body component, the method comprising:
by adding the positive electrode active material to the water so that the slurry contains the positive electrode active material at a concentration of 50 g/L;
maintaining a state where the slurry is stirred for 30 minutes; and
obtaining the slurry pH by measuring the pH of the slurry with a “pH meter” in the state where the slurry is stirred.
|