CPC C09K 8/588 (2013.01) [C09K 8/584 (2013.01); E21B 43/20 (2013.01)] | 26 Claims |
1. A method for preparing an inverted polymer solution comprising:
providing a liquid polymer (LP) composition comprising:
one or more water soluble (co) polymers;
one or more hydrophobic liquids;
one or more emulsifier surfactants; and
one or more inverting surfactants;
inverting the LP composition in an aqueous fluid to provide an inverted polymer solution having a concentration of water soluble (co) polymer of from 50 to 15,000 ppm; and
performing an injectivity test on the inverted polymer solution in which two pore volumes of the inverted polymer solution are injected into a Bentheimer sandstone core at a flow rate of 0.5 ml/min at a temperature of 31° C., and a pressure drop for the inverted polymer solution reaches a steadystate; and
wherein the inverted polymer solution is used in an enhanced oil recovery (EOR) operation.
|