CPC C08L 1/286 (2013.01) [A23K 20/163 (2016.05); A23L 2/52 (2013.01); A23L 29/262 (2016.08); A61K 8/04 (2013.01); A61K 8/731 (2013.01); A61K 9/10 (2013.01); A61K 47/38 (2013.01); A61Q 19/007 (2013.01); C08J 3/07 (2013.01); C09D 7/43 (2018.01); D21H 17/26 (2013.01); A23V 2002/00 (2013.01); A61K 2800/48 (2013.01); C08L 2201/54 (2013.01)] | 4 Claims |
1. A method for producing a dispersion composition, comprising
step 1 of preparing a mixture comprising a carboxymethyl cellulose having a degree of carboxymethyl substitution of 0.20 or more and having a degree of crystallization of cellulose type I of 50% or more, and a water-based medium, and
step 2 of subjecting the mixture obtained in step 1 to stirring at a rotational speed of 8000 to 15000 rpm for 1 minute or more, thereby obtaining a dispersion composition, wherein
the carboxymethyl cellulose in the dispersion composition has a median diameter of 10.0 to 150.0 μm; and
wherein the dispersion composition has a viscosity (6 rpm, 25° C.) of 1000 mPa·s to 30000 mPa·s at a solid content of the carboxymethyl cellulose of 1% (w/v).
|