1. A production method for a core-shell porous silica particle, the method comprising:
(a) preparing an aqueous solution containing a non-porous silica particle, a cationic surfactant, a basic catalyst, and an alcohol;
(b) adding a silica source to the aqueous solution to form a shell precursor on a surface of the non-porous silica particle;
(c) removing the cationic surfactant from the shell precursor and forming a porous shell;
(d) preparing an aqueous solution containing a porous silica particle resulting from the forming the porous shell, a cationic surfactant, a basic catalyst, and an alcohol;
(e) adding a silica source to the aqueous solution to form a shell precursor on a surface of the porous silica particle; and
(f) removing the cationic surfactant from the shell precursor and forming a porous shell; wherein
the steps (d) to (f) are further repeated one to three times, in which case the “forming the porous shell” in step (d) refers to the “forming a porous shell” in step (f).
|