CPC B32B 17/10 (2013.01) [B32B 7/12 (2013.01); B32B 17/10018 (2013.01); B32B 17/10091 (2013.01); B32B 17/10137 (2013.01); B32B 17/10165 (2013.01); B32B 17/10174 (2013.01); C09D 175/04 (2013.01); C09D 183/04 (2013.01); B32B 2250/02 (2013.01); B32B 2307/412 (2013.01); B32B 2307/536 (2013.01); B32B 2307/558 (2013.01); B32B 2307/732 (2013.01); B32B 2457/20 (2013.01); Y10T 428/31598 (2015.04); Y10T 428/31663 (2015.04)] | 11 Claims |
1. A glass article, comprising:
an ultra-thin glass layer;
an optically transparent adhesive layer disposed on the ultra-thin glass layer; and
an optically transparent polymeric hard-coat layer disposed on the optically transparent adhesive layer, wherein the optically transparent polymeric hard-coat layer is a silsesquioxane polymer layer, an aliphatic hexafunctional urethane acrylate layer, or an aromatic hexafunctional urethane acrylate layer and the optically transparent polymeric hard-coat layer comprises:
a pencil hardness of 8H or more, and
a thickness in a range of 10 microns to 120 microns,
wherein the glass article comprises an impact resistance defined by the capability of the glass article to avoid failure at a pen drop height that is 2 times or more than that of a control pen drop height of the ultra-thin glass layer without the optically transparent polymeric hard-coat layer, wherein the pen drop height and the control pen drop height are measured according to the Pen Drop Test, and
wherein the glass article survives a bend radius of 5 mm or less.
|