| CPC C09J 125/06 (2013.01) [C09J 11/08 (2013.01); C09J 123/06 (2013.01); C08J 3/203 (2013.01)] | 8 Claims |
|
1. A method of making a hot-melt adhesive comprising the steps of:
a. heating an aromatic hydrocarbon process oil to a desired temperature that is below a boiling point of the process oil;
b. adding a polymer consisting of expanded polystyrene to and dissolving the polymer in the heated process oil, wherein the polymer is added and dissolved until the hot-melt adhesive includes substantially equal parts by weight process oil and polymer;
c. cooling the process oil and polymer mixture to room temperature resulting in a solid-form hot-melt adhesive.
|
|
5. A method of making a hot-melt adhesive comprising the steps of:
a. heating a process oil to a desired temperature that is below a boiling point of the process oil;
b. adding expanded polyethylene to and dissolving the expanded polyethylene in the heated process oil, wherein expanded polyethylene is added and dissolved until the hot-melt adhesive includes substantially equal parts by weight process oil and polyethylene;
c. cooling the process oil and polyethylene mixture to room temperature resulting in a solid-form hot-melt adhesive.
|