| CPC C08J 3/126 (2013.01) [B01J 20/24 (2013.01); B01J 20/26 (2013.01); B01J 20/261 (2013.01); B01J 20/262 (2013.01); B01J 20/264 (2013.01); B01J 20/265 (2013.01); B01J 20/28 (2013.01); B01J 20/28016 (2013.01); C08F 2/08 (2013.01); C08F 20/06 (2013.01); C08F 120/06 (2013.01); C08G 65/08 (2013.01); C08J 3/16 (2013.01); C08L 33/26 (2013.01); C08L 101/14 (2013.01)] | 16 Claims |

|
1. An absorbent material comprising water-absorbent resin particles, wherein the water-absorbent resin particles comprise a polymer particle having water absorption properties; and a coating layer that coats at least a part of a surface of the polymer particle and contains a water-insoluble component that is at least one selected from the group consisting of polyolefins, polyurethanes, and acid-modified products thereof,
the water-absorbent resin particles have a water absorption rate by a Vortex method of 55 seconds or more,
the water-absorbent resin particles have a water retention amount of physiological saline of 35 g/g to 60 g/g, and
the water-absorbent resin particles have a contact angle with 0.9% by mass saline at 25° C.±2° C. of 100 degrees or larger and 130 degrees or smaller.
|