| CPC H01M 4/667 (2013.01) [H01M 4/134 (2013.01); H01M 4/38 (2013.01); H01M 4/483 (2013.01); H01M 4/661 (2013.01); H01M 4/663 (2013.01); H01M 4/668 (2013.01); H01M 4/747 (2013.01); H01M 10/054 (2013.01); H01M 2004/021 (2013.01); H01M 2004/027 (2013.01)] | 8 Claims |

|
1. A preparation method of a composite current collector for a zinc secondary battery, comprising the following steps:
1) disposing a layer of carbon cloth between two layers of zinc mesh, each layer of the zinc mesh being a composite zinc mesh, and mesh pores of the zinc mesh being filled with tin, thermally pressing the two layers of zinc mesh with the carbon cloth, and rolling the two layers of zinc mesh with the carbon cloth to obtain a pressed zinc mesh, a reduction rate of the two layers of zinc mesh during rolling being within a range of 10-50%;
2) soaking the pressed zinc mesh in a graphene dispersion, then taking out and drying the pressed zinc mesh after soaking; and
3) coating two surfaces of the dried pressed zinc mesh with a conductive paste and drying the coated zinc mesh to obtain the composite current collector for the zinc secondary battery, the conductive paste containing a conductive polymer.
|