| CPC C09K 8/604 (2013.01) [C10G 71/00 (2013.01); C09K 2208/28 (2013.01); C10G 2300/4075 (2013.01)] | 14 Claims |
|
1. A method of producing a solid drag reducing additive, comprising:
forming an emulsified polymer mixture from at least one polar monomer by emulsion polymerization;
disrupting the emulsified polymer mixture by adding a demulsifier and an anti-blocking agent to form the solid drag reducing additive, wherein the demulsifier is selected from the group consisting of C3-C8 ketones and aldehydes;
isolating the solid drag reducing additive;
drying the solid drag reducing additive to 10 wt % or less of water; and
forming a slurry or suspension by adding a carrier fluid to the solid drag reducing additive in a range of about 10 wt. % to about 50 wt. %.
|