| CPC C01D 15/04 (2013.01) [B01J 39/02 (2013.01); B01J 39/10 (2013.01); B01J 49/53 (2017.01)] | 2 Claims |

|
1. A method for producing a lithium-containing solution, comprising:
an adsorption step of bringing a lithium adsorbent obtained from lithium manganese oxide in contact with a lithium-containing solution to obtain post-adsorption lithium manganese oxide;
an eluting step of bringing the post-adsorption lithium manganese oxide in contact with an acid-containing solution to obtain an eluted solution; and
a manganese oxidation step of oxidating manganese by adding an oxidant and a pH adjuster to the eluted solution to obtain a lithium-containing solution with a suppressed manganese concentration, wherein
the adsorption step, the eluting step, and the manganese oxidation step are performed in this order, and
the acid-containing solution includes the eluted solution with acid added, and wherein:
in the manganese oxidation step, the oxidant is selected from the group consisting of sodium hypochlorite, sodium chlorite, ozone, and permanganate.
|