Int. Cl. C08K 13/00 (2006.01); C08K 3/04 (2006.01); C08K 3/26 (2006.01); C08K 11/00 (2006.01); F16G 1/10 (2006.01); F16G 1/28 (2006.01); F16G 5/08 (2006.01); F16G 5/20 (2006.01)
CPC C08K 13/00 (2013.01) [F16G 1/10 (2013.01); C08K 3/04 (2013.01); C08K 3/042 (2017.05); C08K 2003/265 (2013.01); C08K 11/00 (2013.01); C08K 2201/001 (2013.01); C08K 2201/005 (2013.01); C08K 2201/006 (2013.01); F16G 1/28 (2013.01); F16G 5/08 (2013.01); F16G 5/20 (2013.01)] 12 Claims
OG exemplary drawing
 
1. A power transmission belt comprising an elastomeric body having an inner section, an outer section, and a load carrying section between the inner and outer sections, at least the inner section being formed from a conductive rubber mixture comprising:
at least one base rubber selected from one or more of ethylene-propylene-diene rubber, acrylonitrile-butadiene rubber, hydrogenated acrylonitrile-butadiene rubber, natural rubber, and/or styrene butadiene rubber;
25 phr to 100 phr of non-conductive carbon black as a filler, the non-conductive carbon black having a BET surface area of 130 m2/g or less according to ISO 977:2022;
up to 5 phr of graphene as a conductive filler, the graphene having a particle size of between 100 nm to 5 μm, and a specific surface area of less than 200 m2/g;
10 phr to 50 phr of graphite;
2 phr to 30 phr of fiber filler; and
a vulcanizing agent;
wherein the conductive rubber mixture has a resistivity according to ASTM D991-89(2020) of less than 2 MΩ, and
wherein the conductive rubber mixture has an elongation at break of less than 201%.