| CPC D04H 18/04 (2013.01) [B32B 5/022 (2013.01); B32B 5/067 (2021.05); B32B 5/266 (2021.05); B32B 37/0038 (2013.01); B32B 37/0053 (2013.01); D04H 1/4374 (2013.01); D04H 1/49 (2013.01); D04H 1/492 (2013.01); D04H 1/498 (2013.01); B32B 2250/20 (2013.01); B32B 2262/0253 (2013.01); B32B 2262/0261 (2013.01); B32B 2262/0276 (2013.01); B32B 2262/144 (2021.05); B32B 2317/10 (2013.01); B32B 2323/10 (2013.01); B32B 2367/00 (2013.01); B32B 2377/00 (2013.01); D04H 1/4258 (2013.01); D04H 1/4291 (2013.01); D04H 1/4334 (2013.01); D04H 1/435 (2013.01); D10B 2201/24 (2013.01); D10B 2321/022 (2013.01)] | 2 Claims |

|
1. A method for producing a two-ply or three-ply nonwoven comprising:
producing in an inclined wire former a web of wet-laid fibrous material consisting of 70%-95% by weight of pulp and 30%-5% by weight of solvent-spun cellulose fibers; and
selectively forming the two-ply non-woven by performing one of the following steps (A) and (B) or forming the three-ply nonwoven by performing both of the following steps (A) and (B):
(A) depositing a carded nonwoven on the web of wet-laid fibrous material from a card arranged above and downstream in a material transport direction from the inclined wire former; and
(B) introducing a further web on the web of wet-laid fibrous material from either an unwinding station or a further card located upstream of or below the inclined wire former;
wherein each of the carded nonwoven and the further web in steps (A) and (B) consist of 100% by weight of solvent-spun cellulose fibres, or 100% by weight of viscose or 100% by weight of a mixture of solvent-spun cellulose fibres and viscose;
feeding the two-ply or three-ply nonwoven to a hydroentangler for at least one of bonding, entangling and structuring the plys of the two-ply or three-ply nonwoven; and
subsequently drying the two-ply or three-ply nonwoven.
|