CPC C23C 2/06 (2013.01) [B32B 15/01 (2013.01); B32B 15/013 (2013.01); B32B 15/04 (2013.01); B32B 15/043 (2013.01); B32B 15/18 (2013.01); C21D 7/06 (2013.01); C22C 18/00 (2013.01); C22C 18/04 (2013.01); C23C 2/0035 (2022.08); C23C 2/02 (2013.01); C23C 2/285 (2013.01); C23C 2/29 (2022.08); C23C 2/40 (2013.01); C23C 28/02 (2013.01); C23C 28/021 (2013.01); C23C 28/023 (2013.01); C23C 28/025 (2013.01); C23C 28/322 (2013.01); C23C 28/3225 (2013.01); C23C 30/00 (2013.01); C23C 30/005 (2013.01); Y10T 428/12951 (2015.01); Y10T 428/12958 (2015.01); Y10T 428/12972 (2015.01); Y10T 428/12979 (2015.01); Y10T 428/12993 (2015.01); Y10T 428/24942 (2015.01); Y10T 428/24983 (2015.01); Y10T 428/263 (2015.01); Y10T 428/265 (2015.01)] | 6 Claims |
1. A plated steel sheet comprising:
a base steel sheet;
a Zn—Mg—Al-based plating layer provided on at least one surface of the base steel sheet; and
a Fe—Al-based inhibition layer provided between the base steel sheet and the Zn—Mg—Al-based plating layer,
wherein the plating layer includes, by weight, 4 to 10% of Mg and 5.1 to 25% of Al, with a balance of Zn and unavoidable impurities, based on components other than iron (Fe) ,
the plating layer includes a MgZn2 phase at a phase fraction of 24 to 50 wt %, and
an Al single phase is present inside the MgZn2 phase at a ratio of 1 to 30% to a total cross-sectional area of the MgZn2 phase in a thickness direction.
|