| CPC C09D 7/61 (2018.01) [B05D 7/14 (2013.01); C09D 4/00 (2013.01); C09D 5/08 (2013.01); C09D 7/20 (2018.01); C09D 7/63 (2018.01); C09D 7/67 (2018.01); C09D 183/06 (2013.01); B05D 2202/10 (2013.01); C08K 3/36 (2013.01); C08K 2201/005 (2013.01)] | 12 Claims |
|
1. A solution composition for treating a surface of a steel sheet comprising:
15 to 50 wt % of colloidal silica;
20 to 60 wt % of alkoxy silane;
1 to 40 wt % of a solvent;
0.01 to 1.00 wt % of an acidity regulator;
5 to 15 wt % of an acrylate-based monomer;
0.1 to 3.0 wt % of a metal chelate curing agent; and
5 to 50 wt % of an adhesion improver including a backbone formed of siloxane bonds,
wherein the adhesion improver is a silicone resin,
wherein a ratio of silicon dioxide in the adhesion improver is 20 to 80 mol %, and
wherein a weight average molecular weight of the adhesion improver is 300 g/mol to 30,000 g/mol.
|