| CPC A61K 33/38 (2013.01) [A61K 9/10 (2013.01); B01J 13/0043 (2013.01); B22F 1/0545 (2022.01); B22F 9/24 (2013.01); B22F 2301/255 (2013.01); B22F 2304/054 (2013.01)] | 8 Claims |

|
1. A method of producing a highly stable concentrated dispersion of silver nanoparticles, comprising the steps of:
dissolving a combination of a reducing dispersant and co-dispersant in deionized water to form a first solution, wherein the co-dispersant is sodium alginate;
adding silver oxide to the first solution to form a slurry;
mixing the slurry with a basic solution to form an alkaline basic slurry; and
heating the alkaline basic slurry to yield highly uniform silver nanoparticles wherein no silver nanoparticle is larger than 25 nm.
|