| CPC C03C 17/25 (2013.01) [C03C 17/008 (2013.01); C03C 17/326 (2013.01); C03C 2217/228 (2013.01); C03C 2217/76 (2013.01); C03C 2217/77 (2013.01); C03C 2218/31 (2013.01); C03C 2218/32 (2013.01)] | 13 Claims |

|
1. A water-repellent-film-attached glass article comprising:
a glass substrate; and
a water-repellent film on the glass substrate, wherein
the water-repellent film includes cerium oxide as a main component of the water-repellent film,
the water-repellent film has a surface on which the cerium oxide is exposed,
a porosity of the water-repellent film is 40% or more,
a visible reflectance for visible light incident on the glass article from a side on which the water-repellent film is arranged is 10% or less,
a contact angle of water on the surface of the water-repellent film is 75° or greater, and
the contact angle is 75° or greater after the glass article is exposed to a thermal treatment at 760° C. for 4 minutes.
|