CPC H01M 4/5825 (2013.01) [C01B 25/45 (2013.01); H01M 4/366 (2013.01); H01M 4/381 (2013.01); H01M 4/587 (2013.01); H01M 10/0436 (2013.01); H01M 10/054 (2013.01); C01P 2002/52 (2013.01); C01P 2002/72 (2013.01); C01P 2004/03 (2013.01); C01P 2004/04 (2013.01); C01P 2004/24 (2013.01); C01P 2004/80 (2013.01); C01P 2006/40 (2013.01); H01M 2004/021 (2013.01); H01M 2004/028 (2013.01)] | 20 Claims |
1. A method for preparing a vanadium sodium phosphate positive electrode material, which comprises the following steps:
(1) performing a reaction in which an aqueous solution containing a vanadium source reacts with a phosphorus source, a reducing agent, a sodium source, and a carbon source; wherein the reaction comprises: the aqueous solution containing the vanadium source reacting first with the phosphorus source, and then with the reducing agent; or, the aqueous solution containing the vanadium source reacting first with the reducing agent and then with the phosphorus source;
(2) obtaining a reaction solution from step (1), drying and calcining the reaction solution.
|