CPC H01M 4/0435 (2013.01) [H01M 4/0404 (2013.01); H01M 4/485 (2013.01); H01M 4/505 (2013.01); H01M 4/525 (2013.01); H01M 4/58 (2013.01); H01M 4/623 (2013.01); H01M 4/662 (2013.01); H01M 10/0525 (2013.01)] | 14 Claims |
1. A method for producing a dry film, in which
a dry powder mixture is processed into the dry film by a rolling device having a first roll and a second roll, wherein
the first roll has a higher rotational peripheral speed than the second roll and the dry film is supported on the first roll,
wherein a ratio of the rotational peripheral speed of the first roll to the rotational peripheral speed of the second roll of 10:5 to 10:1 is maintained, and
wherein the dry powder mixture contains polytetrafluoroethylene.
|