CPC C08L 9/06 (2013.01) [B60C 1/0016 (2013.01); C08K 3/04 (2013.01); C08K 3/22 (2013.01); C08K 3/36 (2013.01); C08K 5/01 (2013.01); C08K 5/548 (2013.01); C08L 93/04 (2013.01); B60C 2200/04 (2013.01); C08K 2003/2227 (2013.01); C08K 2201/006 (2013.01); C08L 2205/02 (2013.01)] | 19 Claims |
1. A rubber composition comprising:
70 phr to 95 phr of a solution polymerized styrene butadiene rubber having a glass transition temperature within a range of −20° C. and −45° C.;
5 phr to 30 phr of at least one diene based rubber selected from at least one or more of natural rubber, synthetic polyisoprene, polybutadiene rubber and another styrene butadiene rubber;
95 phr to 200 phr of filler comprising:
i) 50 phr to 100 phr of silica,
ii) 40 phr to 70 phr of carbon black, and
iii) 5 phr to 30 phr of an inorganic metal hydroxide;
40 phr to 80 phr of plasticizer comprising a hydrocarbon resin having a softening point within a range of 80° C. to 130° C.
|