CPC C08G 73/1071 (2013.01) [B29C 41/003 (2013.01); B29C 41/46 (2013.01); C01B 32/205 (2017.08); C08J 5/18 (2013.01); C08K 3/32 (2013.01); C09K 5/14 (2013.01); H05K 7/2039 (2013.01); B29K 2079/08 (2013.01); B29K 2509/02 (2013.01); B29L 2007/008 (2013.01); C01P 2006/32 (2013.01); C08J 2379/08 (2013.01); C08K 2003/325 (2013.01)] | 14 Claims |
1. A method for manufacturing a polyimide film for graphite sheets, comprising:
mixing an organic solvent, a diamine monomer and a dianhydride monomer to prepare a polyamic acid solution;
adding a dehydration agent, an imidization agent and a catalyst to the polyamic acid solution to prepare a precursor composition;
forming a gel film by casting the precursor composition onto a support, followed by drying the precursor composition; and
imidizing the precursor composition through heat treatment of the gel film to form a polyimide film,
wherein the catalyst comprises a first catalyst having a linear structure and a second catalyst having a ring structure,
the second catalyst being present in an amount of 10 mol % to 30 mol % based on the total moles of the first catalyst and the second catalyst.
|