US 12,303,611 B2
Liquid dressing for promoting wound healing
Liangfang Wang, Shandong (CN); Kui Zhao, Shandong (CN); Haitao Qiao, Shandong (CN); and Kai Wang, Shandong (CN)
Assigned to ZIBO LEYOUYOU AGRICULTURAL TECHNOLOGY CO., LTD., Shandong (CN)
Appl. No. 18/708,606
Filed by ZIBO LEYOUYOU AGRICULTURAL TECHNOLOGY CO., LTD., Shandong (CN)
PCT Filed Sep. 20, 2023, PCT No. PCT/CN2023/120061
§ 371(c)(1), (2) Date May 9, 2024,
PCT Pub. No. WO2024/078282, PCT Pub. Date Apr. 18, 2024.
Claims priority of application No. 202211237037.7 (CN), filed on Oct. 10, 2022.
Prior Publication US 2024/0416001 A1, Dec. 19, 2024
Int. Cl. A61L 26/00 (2006.01)
CPC A61L 26/0004 (2013.01) [A61L 26/0066 (2013.01); A61L 2300/10 (2013.01); A61L 2300/21 (2013.01); A61L 2300/41 (2013.01); A61L 2300/412 (2013.01)] 3 Claims
 
1. A liquid dressing for promoting wound healing, consisting of, in percentage by weight:
1% to 2% of monomeric silicic acid and 98% to 99% of distilled water;
wherein the monomeric silicic acid is Si(OH)4;
wherein the liquid dressing for promoting wound healing is prepared by a method comprising the following steps:
step 1 of sequentially adding the monomeric silicic acid and the distilled water into a reaction kettle according to the composition ratio, and controlling a temperature to a range from 120° C. to 150° C.;
step 2 of performing a stir in the reaction kettle, and keeping the temperature at 100° C. for 1 to 3 hours after the substances in the reaction kettle are completely dissolved;
step 3 of lowering an internal temperature of the reaction kettle to 50° C., and leaving the mixed liquid after being uniformly mixed to stand; and
step 4 of cooling the mixture obtained in the step 3 to room temperature to obtain the liquid dressing.