CPC C09D 195/00 (2013.01) [C08L 95/00 (2013.01); C09D 7/61 (2018.01); C09D 7/65 (2018.01); C08L 2205/025 (2013.01)] | 28 Claims |
1. A method, comprising:
obtaining an oxidized asphalt;
obtaining a briquette,
wherein the briquette comprises:
a pressurized asphalt shingle waste powder comprising an asphalt shingle waste powder from any form of discarded asphalt shingle, wherein the asphalt shingle waste powder comprises:
limestone, and
5 wt. % to 40 wt. % of a waste asphalt based on a total weight of the asphalt shingle waste powder;
obtaining a phase modifier;
mixing the oxidized asphalt, the briquette, and the phase modifier to form an asphalt mixture,
wherein the asphalt mixture comprises 0.1 wt. % to 10 wt. % of the phase modifier based on a total weight of the asphalt mixture; and
forming a roofing shingle comprising the asphalt mixture.
|