CPC C08J 3/12 (2013.01) [C08K 5/0041 (2013.01); G03G 9/0804 (2013.01); G03G 9/0819 (2013.01); G03G 9/08755 (2013.01); G03G 9/0906 (2013.01); C08J 2367/00 (2013.01)] | 21 Claims |
1. A method for producing resin particles, the method comprising:
a first step of mixing a binder resin and a dye at temperature T that satisfies formula (1) below to thereby obtain a mixture; and
a second step of emulsifying the mixture, a basic compound, a water-based solvent, and a surfactant to thereby obtain a resin base particle dispersion,
wherein the first step is performed before the second step:
the melting point T1 of the dye≤the temperature T≤the thermal decomposition temperature T2 of the binder resin. Formula (1)
|