CPC C03C 25/1065 (2013.01) [C03C 25/20 (2013.01); C03C 25/26 (2013.01)] | 9 Claims |
1. A method for manufacturing an optical fiber by coating a first resin on a glass fiber drawn from a glass base material, and curing the first resin to form a first coating, the method comprising:
causing the glass fiber to travel at a first velocity during a first time period;
increasing the velocity of the glass fiber from the first velocity to a second velocity during a second time period following the first time period; and
maintaining the velocity of the glass fiber at the second velocity during a third time period following the second time period,
wherein TB2/TB1 is greater than 1.0 and less than or equal to 11.0, where TB1 denotes a thickness of the first coating in the increasing, from a start of coating the first resin to a time when the velocity reaches a third velocity that is higher than the first velocity and lower than the second velocity, and TB2 denotes a thickness of the first coating in the maintaining.
|