CPC A41D 13/1192 (2013.01) [A61L 9/20 (2013.01); D06M 10/06 (2013.01); D06M 11/45 (2013.01); D06M 11/83 (2013.01); D06M 23/10 (2013.01); A41D 2500/00 (2013.01); A61L 2209/21 (2013.01); D06M 2101/32 (2013.01)] | 7 Claims |
1. A method of making a UV-C emitting emulsion comprising:
mixing a combination of doped strontium aluminate and a stabilized silver solution in a ratio of 18000:1 to 1600:1 of doped strontium aluminate:stabilized silver solution to form an emulsion;
adding silica to the emulsion to form a mixture; and
heating the mixture for 30-50 seconds at 350° F. to 450° F. (176° C. to 232° C.) at a pressure of 30 psig to 70 psig (207 kPa to 483 kPa).
|