CPC H01M 10/0562 (2013.01) [C01G 25/006 (2013.01); H01M 4/0402 (2013.01); H01M 4/0404 (2013.01); H01M 4/0471 (2013.01); H01M 4/13 (2013.01); H01M 4/139 (2013.01); H01M 4/505 (2013.01); H01M 4/525 (2013.01); H01M 10/0585 (2013.01); B05D 1/26 (2013.01); B05D 1/30 (2013.01); H01M 2004/028 (2013.01); H01M 2300/0068 (2013.01); H01M 2300/0071 (2013.01); H01M 2300/0091 (2013.01)] | 19 Claims |
1. A slurry for forming a lithium ion conducting solid-state electrolyte, the slurry comprising:
a solid electrolyte material, wherein the solid electrolyte material undergoes a loss of lithium during sintering of the solid electrolyte material, and
a dispersant providing a source of lithium ions to address the loss of lithium during sintering.
|