1. Foam particles obtained by foaming a resin composition,
wherein the resin composition comprises a base resin comprising a polycarbonate resin having a glass transition temperature of 140 to 155° C. and an amorphous polyester resin having a glass transition temperature of 100 to 130° C.,
the amorphous polyester comprises a cyclohexanedimethanol-derived unit and a tetramethyl cyclobutanediol-derived unit,
the resin composition has a glass transition temperature of 115 to 131.8° C., and
the resin composition has a melt mass-flow rate of 15 to 25 g/10 min.
|