| CPC H01M 4/0483 (2013.01) [F27B 3/085 (2013.01); H01M 4/131 (2013.01); H01M 4/1391 (2013.01); H01M 10/0525 (2013.01)] | 7 Claims |

|
1. A method of forming an electrode material for use in a battery, the method comprising:
calcining electric arc furnace flue dust so as to recover a metal oxide therefrom, the calcining being at a temperature of 200° C. to 1500° C. for a period of one hour to twenty-four hours, the metal oxide having a purity of between 20% to 99.99%; and
forming the electrode material for use in the battery from the calcined electric arc furnace flue dust without applying any mechanical treatment.
|