| CPC A01N 43/56 (2013.01) [A01N 25/04 (2013.01); A01N 59/20 (2013.01); B27K 3/005 (2013.01); B27K 3/007 (2013.01); B27K 3/0207 (2013.01); B27K 3/08 (2013.01); B27K 3/22 (2013.01); B27K 3/343 (2013.01); B27K 3/38 (2013.01); B27K 3/42 (2013.01); B27K 3/52 (2013.01); B27K 5/0055 (2013.01); B27K 3/163 (2013.01); B27K 3/20 (2013.01); B27K 3/30 (2013.01); B27K 2240/20 (2013.01)] | 25 Claims |
|
1. A wood preservative composition for making a wood or wood product resistant to fungal decay, the wood preservative composition comprising:
an aqueous carrier;
a copper component, wherein the copper component is micronized; and
penflufen,
in a copper:penflufen weight ratio in a range of 5:1 to 200:1,
wherein the wood preservative composition comprises less than 5% by weight of alkanolamines based on a total weight of the wood preservative composition.
|