CPC B27K 3/34 (2013.01) [B27K 3/0214 (2013.01); B27K 3/08 (2013.01); C09D 15/00 (2013.01); B27K 2240/20 (2013.01)] | 8 Claims |
1. A method of treating wood with natural solution to provide enhanced weathering protection and heightened decay hazard ratings comprising:
drying the wood in a kiln, removing water from the wood, forming pre-treated wood;
preparing the natural solution by mixing bio-diesel oil with hemp seed oil;
wherein the solution is comprised of 100% of biodiesel and hemp seed oil;
disposing the solution in a retort cylinder;
placing the pre-treated wood into an interior of the retort cylinder;
sealing the retort cylinder;
the retort cylinder applying pressure to the pre-treated wood within the interior of the retort cylinder;
the pressure impregnating the wood with the solution;
the pressure covering an exterior of the wood with the solution, forming treated wood;
opening the retort cylinder;
removing the treated wood; and
drying the treated wood.
|