| CPC C08L 33/08 (2013.01) [C08K 5/175 (2013.01); C08K 5/42 (2013.01)] | 5 Claims |

|
1. A method for stabilizing a water conditioning agent into a stable solid composition comprising:
combining a water conditioning agent comprising from 22 wt-% to 26 wt-% of a chelant water conditioning agent comprising methylglycinediacetic acid (MGDA) and from 49 wt-% to 51 wt-% of a polycarboxylic acid polymer, copolymer and/or terpolymer (or salts thereof), and from 7.5 wt-% to 10 wt-% of a stabilizing surfactant comprising an amine oxide amphoteric surfactant to form a stable solid composition;
wherein the stable solid composition is pressed, cast or extruded;
wherein the stable solid composition does not comprise sodium carbonate; and
maintaining the stable solid composition, wherein the stable solid composition has less than 5% change in thickness and diameter when heated to a temperature of 40° C. for two weeks with 65% humidity.
|